General notes:
| State | 50% cold reduction |
| Density | 8.4 g/cm3 |
| Hardness, Vickers | 260 HV |
| Tensile strength, ultimate | 925 MPa |
| Tensile strength, yield | 485 MPa |
| Elongation, break | 50% |
| Modulus of elasticity | 208 GPa |
| Coef. of lin. therm expansion | 12.8 E-6/°C | 25°C-100°C |
| Coef. of lin. therm expansion | 13.4 E-6/°C | 25°C-300°C |
| Specific heat capacity | 0.41 J/(g∙K) | |
| Thermal conductivity | 10 W/(m∙K) | |
| Continuous use temperature | 600°C | |
| Max service temperature, air | 980°C |
| Resistivity | 1.29 E-4 Ohm.cm |